John: I have seen dies resurfaced nicely on a horizontal mill, using a
fly-cutter. Grant
-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net]On Behalf Of Demon Buddha
Sent: Tuesday, June 06, 2006 7:13 PM
To: Sponsored by ABANA
Subject: Re: [TheForge] Repairing power hammer dies
JOHN CHOBRDA wrote:
> Gentleman,
>
> I am in the process of rebuilding a little giant hammer that I
> recently acquired. One of my problems is that some where the hammer was
> used I guess for texturing, as the dies (upper and lower) have a bunch of
> small shallow depressions in them. Has any one any experience resurfacing
> dies. I do not want to grind them because some of the dimples are fairly
> deep. Any suggestions are greatly appreciated.
Just fill them. I suppose you could use a hardface rod, but I don't
think it would be necessary. The dies are probably 4140 or similar for
toughness. They don't have to be very hard. Maybe 7018 would suffice?
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
More information about the TheForge
mailing list