I'd tell you but,I'm having a senior moment. I got the plans from the ABANA
web site.It cost about $1000 to build but I didn't spend time scrounging
the steel. The air cylinder and valving cost $400-$500 because I was
playing around with the valving sceam .
At 06:22 AM 6/5/2006 -0400, you wrote:
>Kim, what kind of power hammer did you build?
>
>Ron Childers
>
>
>-----Original Message-----
>From: theforge-bounces at mailman.qth.net
>[mailto:theforge-bounces at mailman.qth.net] On Behalf Of kim george
>Sent: Sunday, June 04, 2006 11:37 PM
>To: Sponsored by ABANA
>Subject: Re: [TheForge] Anybody out there?
>
>On one I had a couple of layers that wouldn't weld .I peeled the top one
>off , spread and cleaned the interior one and got it to weld,drew it out
>and ground one side,cut and folded. It welded right up. The main problem
>was that I didn't have a striker then and have since then built a power
>hammer. It's real nice not having to reattach my arm after every session.
>:-)))
>
>At 09:15 AM 6/4/2006 -0800, you wrote:
> >I used to hate it when a job proved more stubborn than me. Then some 29
> >years ago I went to work for the state of AK. and learned the futility of
> >ambition. Now if a job looks to be very stubborn I give it to one of the
> >new guys. <grin>
> >
> >Seriously though, what was it about the billets you had trouble with Kim?
> >
> >I know I've tried welding things I discovered later weren't particularly
> >weldable without going to special and or extreme measures.
> >
> >Frosty
> >-------------------------------
> >If it ain't forged
> >it ain't real.
> >Wrought iron is.
> >The FrostWorks
> >
> >Meadow Lakes, AK.
> >
> >http://www.artmetalradio.com/
> >
> >From: "kim george" <klgeorge at kent.edu>
> >
> >
> >>I've been trying to breath some life into some billets that had proven
> >>stubborn to weld 2or 3 years ago.
> >>
> >
> >_______________________________________________
> >Manage membership or unsubscribe at:
> >http://mailman.qth.net/mailman/listinfo/theforge
> >theforge mail list group photo site is
> >http://www.photoaccess.com
> >Login: blacksmithblacksmith at hotmail.com
> >password: anvil
> >___________
> >
> >
>
>Kim George
>
> "Why for you burry me in cold,cold ground?" Taz
>
>
>_______________________________________________
>Manage membership or unsubscribe at:
>http://mailman.qth.net/mailman/listinfo/theforge
>theforge mail list group photo site is
>http://www.photoaccess.com
>Login: blacksmithblacksmith at hotmail.com
>password: anvil
>___________
>
>
>
>_______________________________________________
>Manage membership or unsubscribe at:
>http://mailman.qth.net/mailman/listinfo/theforge
>theforge mail list group photo site is
>http://www.photoaccess.com
>Login: blacksmithblacksmith at hotmail.com
>password: anvil
>___________
Kim George
"Why for you burry me in cold,cold ground?" Taz
More information about the TheForge
mailing list