Kim, what kind of power hammer did you build?
Ron Childers
-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of kim george
Sent: Sunday, June 04, 2006 11:37 PM
To: Sponsored by ABANA
Subject: Re: [TheForge] Anybody out there?
On one I had a couple of layers that wouldn't weld .I peeled the top one
off , spread and cleaned the interior one and got it to weld,drew it out
and ground one side,cut and folded. It welded right up. The main problem
was that I didn't have a striker then and have since then built a power
hammer. It's real nice not having to reattach my arm after every session.
:-)))
At 09:15 AM 6/4/2006 -0800, you wrote:
>I used to hate it when a job proved more stubborn than me. Then some 29
>years ago I went to work for the state of AK. and learned the futility of
>ambition. Now if a job looks to be very stubborn I give it to one of the
>new guys. <grin>
>
>Seriously though, what was it about the billets you had trouble with Kim?
>
>I know I've tried welding things I discovered later weren't particularly
>weldable without going to special and or extreme measures.
>
>Frosty
>-------------------------------
>If it ain't forged
>it ain't real.
>Wrought iron is.
>The FrostWorks
>
>Meadow Lakes, AK.
>
>http://www.artmetalradio.com/
>
>From: "kim george" <klgeorge at kent.edu>
>
>
>>I've been trying to breath some life into some billets that had proven
>>stubborn to weld 2or 3 years ago.
>>
>
>_______________________________________________
>Manage membership or unsubscribe at:
>http://mailman.qth.net/mailman/listinfo/theforge
>theforge mail list group photo site is
>http://www.photoaccess.com
>Login: blacksmithblacksmith at hotmail.com
>password: anvil
>___________
>
>
Kim George
"Why for you burry me in cold,cold ground?" Taz
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
More information about the TheForge
mailing list