On Fri, 30 Jun 2006, James Binnion wrote:
> Terry,
>
> Dan is absolutly correct.
>
i really do not care whether dan is or or is not correct.
his condescending attitude is a turn off.
>
> Copper and iron are soluble in each other.
> I guarantee your steel crucibles will alloy with the copper
> and it will dissolve the crucible in short order.
>
define 'short order'.
are we talking catastrophic failure in a single use?
are we talking catastrophic failure in a two uses?
>
> Iron based crucibles are somewhat ok for aluminum and lower temp
> metals but no good for higher temp metals.
>
i have silicon carbide crucibles for aluminum and brass.
>