Here's a link to a similar sculpture community discussion group thread. It
seems Lincolnweld LA-75 is another alternative. Try "Googling" things like
"Corten welding rod" and the like and you'll get lots of hits.

Dan

-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of G. Watts
Sent: Wednesday, January 25, 2006 6:10 PM
To: Sponsored by ABANA
Subject: RE: [TheForge] Corten Welding Filler

Ray,
ESAB recommends E8018-C3...never tried it, but I'm pretty sure I've seen
that rod referenced for Corten before.
http://www.esabna.com/html/techtip2.cfm

If you have thicker material that requires multi-pass welds, you can fill
with 7018, then cover with the higher dollar 8018-C3 for color matching.
Hope this helps.
George.


-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net]On Behalf Of debmiller at fuse.net
Sent: Wednesday, January 25, 2006 9:54 AM
To: Sponsored by ABANA
Subject: [TheForge] Corten Welding Filler


Hey People,

Probably an old question but here goes.

I am working on confirming a good stick or MIG filler for welding a large
scale corten sign for a client. They do not want the seams to be blatanly
obvious.

Once assembled we are looking at bead blasting the entire surface to attempt
to get as uniform as possible patina. 

Recommendations on spec for rod or wire??

Ray Miller
Cincinnati
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login:  blacksmithblacksmith at hotmail.com
password:  anvil
___________


_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login:  blacksmithblacksmith at hotmail.com
password:  anvil
___________





More information about the TheForge mailing list