[TheForge] nail header question

Stephen Viola stephen.viola at gmail.com
Sun Jan 22 14:30:03 EST 2006


Actually this has just been a question recently addressed locally.
There was a group of us messing about forging nails, and it seemed
that the group was split as to which way to place the nail. I was for
the [/ \] style although there were others who preferred the [\ /]
way. Both seemed to work fine and none of us had any difficulties. So
although there might be a right way of doing things I doubt if any
blacksmith here will tell you not to do it if it works for you. So we
agreed to disagree!

Wombat

On 1/22/06, Steven.Walker at its.state.ms.us <Steven.Walker at its.state.ms.us> wrote:
>
>    >If  this  is  one  of  those "domed" hea ders, are you sure you have
>    turned it
>    >right  side  up?     Some  peo  ple  think  you make the head in the
>    depression but
>    >that's wrong. &nbs p;You make the head over the dome.
>    Yeah, that's what I'm doing. I'm using it with the dome at the top and
>    the  depression at the bottom.  Not really sure how someone could even
>    attempt to make the head in the depression side. I guess the hole just
>    got punched (tapered) backwards.
>    Confidentiality  Note: The information contained in this email and/or
>    document(s)  attached  is for the exclusive use of the individual nam   ed  above and may contain confidential, privileged and non-disclosable
>    i  nformation.  If you are not the intended recipient, you are hereby
>    noti   fied   that   you   are   strictly  prohibited  from  reading,
>    photocopying,  d  istributing  or  otherwise using this e-mail or its
>    contents  in  any  way.  If  y  ou have received this transmission in
>    error, please notify me immediate ly.
>    _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
>
>
>


More information about the TheForge mailing list