[TheForge] Tungsten

Ralph Sproul brhlbsmt at mcttelecom.com
Sun Jan 1 22:10:39 EST 2006


Hochewa, Thanks for the reply - and I definitely second Steve's question in
what alloys might be considered good for this slit/drift process in a press?

Ralph

-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net]On Behalf Of Steve Smith
Sent: Sunday, January 01, 2006 10:25 AM
To: Sponsored by ABANA
Subject: Re: [TheForge] Tungsten


Thanks for the details, Hochewa. It does seem like difficult stuff for
blacksmiths to work with. From what you're saying, it wouldn't work well.

The problem we're really aiming at with the tungsten is slitting and
drifting large pieces in a hydraulic forging press. The tools we've
tried have a marked tendency to weld in the hole. Pretty ideal
conditions for welding it seems to me--steady pressure, scraping to
clean off any impurities (like anti-seize). What alloy would be least
likely to weld, and will it really be much improvement over other alloys?

Steve

Hochewa at aol.com wrote:
> To  All,
>      Does anyone have a source for 3/4, 7/8, or 1"  round Tungsten.  it is
a
> "refractory metal" .
>
> Typically, Tungsten begins its life as a 1" square bar made from  powder.
> We use tungsten as an alloying element at work.   If we get lump Tungsten
in
> and the pieces are too big, we just hit them with a  hammer and the
smaller
> pieces work just fine.  It is brittle to say the  least.
> Being a refractory metal means that it has a high melting point.  It  does
> not mean suitable for use at high temperatures even though as an alloying
> element, it gives better high temperature properties.  One of the
disturbing
> characteristics of refractory metals is that they have very poor
oxidation
> resistance at relatively low temperatures.  Tungsten and  Molybdenum
oxidize very
> rapidly at 1500*F and their oxides are  volatile.
> It's not cheap, it oxidizes easily and you forge it at really white  heat.
> There are better materials available.
>
> Hochewa
>
>
>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
>
>
>
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login:  blacksmithblacksmith at hotmail.com
password:  anvil
___________




More information about the TheForge mailing list