Seems I spoke too soon on the availability of an agent that reacts with zinc
to blacken.(I just looked at Triple S's website) I still stand by the rest
of the message. cheers.......
----- Original Message -----
From: "Woolley" <wjec at verizon.net>
To: "Sponsored by ABANA" <theforge at mailman.qth.net>
Sent: Tuesday, February 28, 2006 10:15 PM
Subject: Re: [TheForge] searching for black-galvanized chain
> Brian,
>
> IMO if this is an exterior job, you are definitely barking up the wrong
> tree trying to use patinizing chemicals such as you would find from Triple
> S, Sur Fin or Sculpt Nouveau. If they want a rust resistant finish, why
> not go with a good paint? Or if you want to galvanize first, just make
> sure you choose a paint that won't react with the zinc etc. If you try to
> patinate with a blackening agent such as Birchwood -Casey after you
> galvanize I don't think it will even work .Consider that you would need to
> clear coat to seal as well. Sculpt Nouveau makes material that you can use
> to patinate almost any substrate but it is a coating that can be chipped
> off, not what I think you are looking for. Don't forget the time and
> effort to experiment with whatever chemicals you choose. In my experience
> using blackening agents and the like there was a learning curve no matter
> what info you get from the makers of the material and were always used for
> interior pieces. My 2 cents. Good luck.
>
> Regards,
> Bill Woolley
>
>
>>I am doing a repair job on a local, old cemetery. The
>> commission wants me to run very rust-resistant chain
>> between granite posts. The chain will be 3/8" stock,
>> 250' long. So the question is...
>>
>> I was hoping to find a place that sells
>> black-galvanized chain but was unable to find any via
>> the web. I called local galvanizers but the cost was
>> going to be very expensive. So does anyone know where
>> I can get "pre-made" black galvanized chain?
>>
>> If I cant find anyplace, I plan on using regular
>> silver-galvanized and dye it with "Triblack G" which
>> is designed to patina galvanize black. Does anyone
>> have good/bad experience with this stuff?
>>
>> Alternately if I could find some plastic coated stuff
>> like McMaster-Carr sells in black (all they have is
>> green) that would probably work too.
>>
>>
>> Thanks alot for your help,
>> Brian
>> -frozen in Massachusetts!
>>
>> __________________________________________________
>> Do You Yahoo!?
>> Tired of spam? Yahoo! Mail has the best spam protection around
>> http://mail.yahoo.com
>> _______________________________________________
>> Manage membership or unsubscribe at:
>> http://mailman.qth.net/mailman/listinfo/theforge
>> theforge mail list group photo site is
>> http://www.photoaccess.com
>> Login: blacksmithblacksmith at hotmail.com
>> password: anvil
>> ___________
>>
>>
>>
>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
More information about the TheForge
mailing list