[TheForge] Forging Bronze

Bill Roberts robertsb at pig.net
Thu Feb 2 10:04:42 EST 2006


Hi David,
I've always used mig or tig. You can get spools of silicon bronze  
wire, and silicon bronze tig rod. Gives a better color match, when  
it's time for the patina. FWIW.

Bill Roberts
www.CustomDesignMetalArts.com