To each his own, but forging that ellipse over a cone mandrel struck me
as pretty easy.

I'd say, a cone or cylinder mandrel for one ellipse,  a jig for 100.

Bruce
NJ

>>> frosty at customcpu.com 11/30/2006 11:44 PM >>>

From: "April & Bill Clemens" <newky2 at dejazzd.com>



>
>
> Bruce and All,
>
> I also forged an ellipse using a cone.  Posted 
> pictures in album ellipse
> 2006...
>
> It works but with some fixtures to hold the ellipse 
> on the cone I think  I
> could forge one by hand to match a drawing on a 
> layout table much quicker.
> If I had to  make 100...
>
> Bill
>
>


Yeah, match a drawing for one or three but make a 
proper jig for 100.

Frosty
-------------------------------
If it ain't forged
it ain't real.
Wrought iron is.
The FrostWorks

Meadow Lakes, AK.

http://www.artmetalradio.com/ 

_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge 
theforge mail list group photo site is
http://www.photoaccess.com 
Login:  blacksmithblacksmith at hotmail.com 
password:  anvil
___________




More information about the TheForge mailing list