Michael wrote:

>Yes and no. What you left out of the plan is complete drying time followed
>by heat curing (at least to red) for the rigidizer. Then complete drying
>time followed by heat curing (at least to red) for the Plistex. Only then
>does the ITC 100 get put on followed by...well, you get the picture, right?
>Mikey 
>