SO...

Put in the first layer of K-wool against tank , only need to spray 
exposed edge.

The inner layer I will install in forge, then spray .25 -.50 " into 
surface of  K-wool.

Apply Plastix  fr900 .50" thick  (mas o menos).

Apply ITC-100 (because I already have some).

Let dry between applications

Thank you one and all
Ken O'Loughlin