I bought the Wilton 225 cold saw about 3 years ago and am very happy with
it. It uses a tool steel blade, cuts at about 60 rpm and has a coolant
system. Very accurate cuts in up to 2x1" stock. Cuts bevels to 45 deg. I
can cut 1x1 square bar in 20 sec. Cost is about $1000 for the saw and $100
for the blade which is resharpenable for about $15. 85 pounds so it can go
to a jobsite, if necessary. Quiet with no abrasive dust. Can't cut
hardened stock though.
-Rick
-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of Justin Fisher
Sent: Sunday, August 27, 2006 6:16 PM
To: 'Sponsored by ABANA'
Subject: [TheForge] Any recommendations on cutoff saws? Brands, etc?
I've decided to add a cutoff saw to my collection, and I am seeking advice:
any brands better/worse than the others?
is the Harbor Freight stuff too junky, or a reasonable alternative?
I know some of you guys are opinionated, so what do you say?
--Justin
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
More information about the TheForge
mailing list