Try A Cut Above;
I used to deal with Klingspor years ago, but have become a
convert ...PF
http://www.acutabove.com/
Ries Niemi wrote:
>
> I have been using Klingspor pretty much exclusively since about 86 or
> so, and I have to agree, its great stuff.
> Particularly their flap discs, which they used to call "mop discs".
> I use the 50 grit on my 4 1/2" grinders- alumina zirconia, they last a
> long time, will cut aggressively or finish smoothly, and cost, in boxes
> of 10, about half of what the welding supply store charges for Walter
> brand.
> I also run their CS411 blue, alumina zirconia abrasives on all my belt
> sanders, and on my 12" disc sander. You can feed 1/2" round into the
> disc, and it just disappears.
>
> ries
>
>
> On Aug 11, 2006, at 8:07 AM, Michael wrote:
>
>>
>> A Klingspor dealer showed up at the recent blacksmith swap meet in
>> Seattle.
>> I have been intending to give an unabashed advertisement for their
>> products
>> every since. Klingspor sells high quality German made grinding and
>> sanding
>> products, with cutting edge design, at Taiwan import prices--that is
>> before
>> the 30% discount for anyone with a business license (the prices fall
>> further
>> if your business uses a lot of the product). All I can say is visit their
>> website and buy what you can before they become better known and their
>> pricing shoots WAY up. This is the best stuff I've ever seen, bar none!
>>
>> There is a local dealer in Seattle now, so there is probably one in every
>> major metropolitan area.
>> Mikey
>>
>>
>>
>>
>> _______________________________________________
>> Manage membership or unsubscribe at:
>> http://mailman.qth.net/mailman/listinfo/theforge
>> theforge mail list group photo site is
>> http://www.photoaccess.com
>> Login: blacksmithblacksmith at hotmail.com
>> password: anvil
>> ___________
>>
>>
>>
> Ries Niemi
> Industrial Artist
>
> http://www.RiesNiemi.com
>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
>
More information about the TheForge
mailing list