The future 2 anvil has the top half made of steel and the lower half out of
aluminum. It has a rubber gasket between the halves and I think that is what
keeps it from ringing. Plus the 2 large bolts holding the halves together. I
have not had any problems with putting dinks in face or edge yet but the
horn had a really sharp point on it when I got it. It does make a great
traveling anvil. It was made for farriers I think.
Info on my Delta future 2 anvil.
Comparable in size to a 155 lb. anvil
52 Rockwell hardness
10" throat
Cone shaped horn
1" hardy 1/2" pritchel
Manufactured with a gasket between the top and bottom, allowing for quiet
operation and quick energy return.
Height 10" Length 27"
Face 4" x 16 1/4"
Base 7"x 15 1/4"