[TheForge] Drilling hard metal

Bruce Freeman FREEMAB at pt.fdah.com
Thu Apr 20 12:44:56 EDT 2006


Why not use the same trick used for drilling rock and glass:  An
abrasive material driven by the end of a copper rod in a drill press. 
Can't get any cheaper than that.  I haven't tried it myself, though.