[TheForge] Re: Kaowool
Mike Porter
michael.a.porter at comcast.net
Sat Apr 15 22:02:27 EDT 2006
Martin,
It is probably stove mortar. Nothing with silica prominently mentioned
(probably is the binder material) is likely to be more than 2300 F.
Mikey
-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of Martin Paietta
Sent: Saturday, April 15, 2006 5:08 PM
To: 'Sponsored by ABANA'
Subject: RE: [TheForge] Re: Kaowool
I was given a bag of AP green castable refractory. I am trying to figure out
the rating of the stuff I have, but it does not say it on the bag. Mike said
I should not waste my time on anything less then 3k for a foundry. The only
thing I can find is Silca cement and a code that says 69E. I know that is
not much, but can anyone tell me what I have?
Thanks
Martin
-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of Jerry Frost
Sent: Saturday, April 15, 2006 4:54 PM
To: Sponsored by ABANA
Subject: Re: [TheForge] Re: Kaowool
A.P.Green have always been special order products in my neighborhood. I
patronize the E.J. Bartells outlet in Anchorage. http://www.ejbartells.com/
I just checked out their product list and had to skim severely! There are a
BUNCH and a search for phosphate refractories returned 76 hits though I
couldn't tell quite which were which. That is of course what the guy behind
the desk is for. <grin>
They have a distributor locator on the site.
Frosty
-------------------------------
If it ain't forged
it ain't real.
Wrought iron is.
The FrostWorks
Meadow Lakes, AK.
http://www.artmetalradio.com/
From: "Chuck Robinson" <robi5515 at bellsouth.net>
> Don't know if it's so nationally, but Harbison Walker is now running
> the A P Green outlets in my area Chuck
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
More information about the TheForge
mailing list