On Apr 4, 2006, at 7:20 PM, Patty Draper/Bill Robertson wrote:
> Does anyone know a supplier that carries really off size stock. I
> have looked for 7/16 flat stock in 3/4 to 1' widths and have been
> unsuccessful with the suppliers I have contacted. And, no, I really
> don't want to forge 12 feet of it down. Bill
>
Have you checked for availability in 1018?
A36 hot rolled is limited on size but 1018 cold rolled has more sizes.
Bob