[TheForge] forging copper?
Rob Fertner
rfertner at cox.net
Tue Sep 27 19:58:44 EDT 2005
Beryllium is highly toxic. I've been told not to forge anything with
beryllium or grind it. It's not worth the risk.
-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of Roy Wilson
Sent: Tuesday, September 27, 2005 6:41 PM
To: Sponsored by ABANA
Subject: Re: [TheForge] forging copper?
======= On 2005-09-27, at 18:22:52 schade wrote: =======
>Is copper electric buss bar okay to forge?
They've got beryllium in the alloy. I wouldn't breathe the smoke,
but I don't know exactly how toxic it is.
"Caesar si viveret, ad remum dareris." - Xanthippos
Roy Wilson - rwilson9 at twcny.rr.com
2005-09-27
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
More information about the TheForge
mailing list