I found a few mentions of sharpening. It looks like Centaur offers a
sharpening for $65. Seems like enough!!
http://www.centaurforge.com/b3bevsharp.html
__________
The "Guru at Anvilfire says...
http://www.anvilfire.com/FAQs/archives/g052004d.htm
Sharpening Shear Blades: (missed that one). That depends on the type of
shear. Long precision metal (paper and other) shears are normally
sharpened on a surface grinder or with a precision sharpening fixture.
This is the only way to produce an absolutely square straight grind.
Often blades from large shears must be sent back to the factory to be
sharpened.
Short shear blades can also be sharpened on a belt grinder with a
table set exactly square. Special shear blades like those for a Beverly
Shear must be ground at a clearance angle. On the Beverly that is 10
degrees. This angle must be very accurate as the blades pass each other
at that angle. To do the job RIGHT requires a special fixture to hold
the curved blades at the correct angle. And folks want to know why one
gets pissed when someone chips their new Beverly Shear blades. . .
After sharpening on a precision grinder the edges have any burr or
wire edge removed by carefully stoning with a fine stone. When
installed the blades are adjusted to have a minimum non-contact
clearance. This is usualy only about .005" (.13mm) and is set using a
feeler guage.
- guru - Wednesday, 05/26/04 23:15:11 EDT
____________________
http://www.weldingweb.com/showthread.php?t=465
BTW a flapdisk and a steady hand does a great job sharpening the
blades as long as they're not to beat up. and keep an eye on the
alignment to ensure burless cuts.
_________
Beverly shear
blades sharpened, $35 plus shipping, bring the
shear to the Folk School or ship the blades to me.
Clay Spencer, 934 Partridge Ln, Murphy, NC
28906 828-837-0708 email: clayms at 2brmemc.net
__________
More information about the TheForge
mailing list