Does anyone know offhand if structural steel (2010? basic hot rolled) can be cryohardened with LN2? The pieces are too thin to heat and superquench. "Caesar si viveret, ad remum dareris." - Xanthippos Roy Wilson - rwilson9 at twcny.rr.com 2005-09-12