MG750
----- Original Message -----
From: "Ron Childers" <munlaw2 at hcsmail.com>
To: "'Sponsored by ABANA'" <theforge at mailman.qth.net>
Sent: Friday, October 28, 2005 11:47 AM
Subject: RE: [TheForge] welding spring steel
> Normalize
>
> -----Original Message-----
> From: theforge-bounces at mailman.qth.net
> [mailto:theforge-bounces at mailman.qth.net] On Behalf Of Wayne
> Sent: Friday, October 28, 2005 9:30 AM
> To: Sponsored by ABANA
> Subject: [TheForge] welding spring steel
>
> I am making a pair of forks to attach to the bucket on my tractor. I
> had some old truck leaf springs that I thought would be ideal. I took
> some of the bend out in the forge and welded them up. I am having
> trouble with the welds breaking. I am a self-taught welder so reading
> up a bit, it appears I should be preheating before welding, but I was
> also wondering what rod I should be using for a better weld. I am
> trying to weld a mild steel spacer between two leaf springs.
>
> thanks
> Wayne
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
More information about the TheForge
mailing list