> Pete,
> What you have just done with your mystery metal is the equivalent of
picking
> up a snake with a rattle on its tail to see if it is poisonous.
> Good luck,
>
> Hochewa
>
> In a message dated 10/24/2005 2:12:31 A.M. Eastern Standard Time,
> artgawk at thegrid.net writes:
>
> Just to double check...anyone know of valve disks of berillium
> copper?
> I got about 80# of big bronze valve disks from a junkyard that
> gets stuff from Vandenburg AFB. Cut some slices off ( took a long
> time to cut with a bandsaw) and it forges a little stiff, but
> nicely enough. No zinc offgassing, heats to a medium red and
> works without problems. unfluxed puddle forms a tough oxide skin.
> Pretty stiff cold.
> I'd guess it is silicon bronze but it seems a bit harder and not
> as red and sticky.
> Am i messing with trouble?...Pete F
>
>
>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
More information about the TheForge
mailing list