[TheForge] steel scrap
Bruce Freeman
FREEMAB at pt.fdah.com
Wed Oct 19 15:52:11 EDT 2005
Why water? Cheap? Nontoxic? Nonflammable?
I was wondering about using some sort of oil instead. The idea would be to leave a protective coat on the metal. May not always be desirable, of course. No oppt'y to try it myself anytime soon...
Bruce
NJ
>>> mrscherm at aol.com 10/19/2005 12:33:04 PM >>>
I've used stone gravel with pretty good success for removing burrs,
rust and corrosion. Put it in with the parts into a rubber bucket
(sometimes add a gallon or two of water) and roll it for few hours. The
parts have to be dried immediately or they rust real quickly.
Michael
___________
More information about the TheForge
mailing list