[TheForge] Wire Cloth

Roy Wilson rwilson9 at twcny.rr.com
Fri Oct 7 16:44:01 EDT 2005


  
======= On 2005-10-07, at 12:32:59 Hufford, David wrote: =======

>   Has  anyone  used  bronze  (as  opposed  to  = steel) wire cloth for a
>   fireplace  screen?   If  so,  any  thoughts  as  =  to the outcome ...
>   appearance, durability, and such.

	I haven't made a screen from it, but I have one here on my fireplace.  About 10-15 years old, sees a lot of use, and looks as good as a new one.


"Caesar si viveret, ad remum dareris." - Xanthippos

Roy Wilson - rwilson9 at twcny.rr.com
2005-10-07