[TheForge] Mystery Metal

Bruce Freeman FREEMAB at pt.fdah.com
Fri Oct 7 08:05:39 EDT 2005


Well, "316" is a common SS.  A little googling reveals that there is a JIS 4316 SS, apparently a welding rod.  JIS is apparently a Japanese standards association:
http://www.garanticelik.com/index.asp?standarts_grades

Whether this is relevant or coincidental, I can't say.

Bruce

>>> jonned at hvc.rr.com 10/6/2005 2:24:29 PM >>>
So, I suppose my mystery metal is actually stainless steel. I was able to 
run a nice fused bead with my tig welder. As I understand it MONEL does not 
weld. Is that correct?

The only thing I am surprised by is the "oxide" on the surface of the bars, 
brownish. NOt what I would expect from Stainless. Also, I sanded the 
surfaces of the 2 small pieces and the area near the weld turned a light 
brown, with no hint of blue or grey.

There is a number stamped near one end, 4316. Does that indicate anything to 
any of you?

Jonathan Nedbor 


_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge 
theforge mail list group photo site is
http://www.photoaccess.com 
Login:  blacksmithblacksmith at hotmail.com 
password:  anvil
___________





More information about the TheForge mailing list