[TheForge] Nasty Slack Tub now sealer
Grant Marcoux
gblacksmith at alamedanet.net
Sat Oct 1 17:56:37 EDT 2005
Ralph: Thanks for the reply....we seem to be on the same page re metal
thickness/weight. The original panel was to be 9 feet wide by 3 feet high.
This panel would feature pierced decorations (cut outs) a la gothic revival.
I had also spoken with my welding supplier about using paste solder in any
gap between panel and frame. He thought this would work, provided you used
a soft (oxygen free) flame to flow the solder into the gap. He suggested a
reducing flame of acetylene and I'm thinking MAPP gas with a soldering tip
on a bernzomatic propane torch...kind of like auto body work. Any thoughts?
-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net]On Behalf Of Ralph Sproul
Sent: Saturday, October 01, 2005 5:04 AM
To: Sponsored by ABANA
Subject: RE: [TheForge] Nasty Slack Tub now sealer
Grant, Sorry for the late reply - but I've been on the road and this was
recieved the day I left. The seam sealer I mention is used in the
automotive industry and auto body shops. It's big thing is it's capilary
action that creeps into seems (of the spot welded sheet metal in
automobiles). It is best used in tight areas where the material sets up and
seals the joint from air and water. If there are a lot of open edges - this
will not work real well.
I've found sheet in the 14 - 10 guage range easy to cut for decorations and
lighting.....but if you have to weld to the middle of it in any way - 3/16
is a way to cut heavy distortion - that seems to be the breaking point of
having enough heat sink to work against. Strictly decorative inset the
panel should be lighter than 3/16.
Never considered solder as a seam sealer - did it work out well?
Ralph
-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net]On Behalf Of Grant Marcoux
Sent: Monday, September 12, 2005 11:10 AM
To: Sponsored by ABANA
Subject: RE: [TheForge] Nasty Slack Tub now sealer
Ralph (or any others): Good advice on the sealer. Question: I'm working
on a gate of 9' length and 6'height, which will have an inset metal panel of
9'x3' I'm planning to decorate the panel with piercings (shapes cut out w/
plasma cutter, leaving negative space openings. I'm thinking of sealing the
edges of the panel, where it mounts inside the gate frame, with lo-melt
solder after MIG welding the panel in place. Any opinions? Also, what
thickness of sheet would you recommend for the 9'x3' panel? Grant l
-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net]On Behalf Of Ralph Sproul
Sent: Monday, September 12, 2005 3:41 AM
To: mspencer at tallships.ca; Sponsored by ABANA
Subject: RE: [TheForge] Nasty Slack Tub
Mike, do yourself a favor - go get the gas and use hard wire, you'll like it
much better. Get the ER70S6 and it will run and flow out real nice for you
on sheet work. Trick with sheet is tack weld all sides/edges, then run
beads - or if real thin and distorting just stich weld to keep distortion
down and use seam sealer(comes in caulking gun and creeps into joint to seal
it - it's what the factory uses - only they spot weld).
Sorry I couldn't make Can-Iron, was really looking forward to meeting you.
I had a killer job going on a water powered sawmill and had to finish it up
before heading out to Minnesota today.
Ralph
-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net]On Behalf Of Mike Spencer
Sent: Monday, September 12, 2005 1:27 AM
To: theforge at mailman.qth.net
Subject: Re: [TheForge] Nasty Slack Tub
> I purchased an old Jack Daniels barrel and after filling it for the first
> time it smelled so good that I almost drank from it.
I once purchased a 50 gal whiskey barrel from the local cider mill and
had 30 gal. of cider put in. Some good cider, my son! I later was
told that the wood of the barrel held about 1 gal of whiskey, so as
the cider equilibrated with the whiskey, I was getting a 30:1 or
better cocktail.
Ob. Smithing: Finally broke down and bought a MIG welder. Don't have
the gas tank yet so I'm using flux core. I figure by the time I've
welded all the patches on my rusty '87 F-150, I'll know how to use the
thing.
- Mike
--
Michael Spencer Nova Scotia, Canada .~.
/V\
mspencer at tallships.ca /( )\
http://home.tallships.ca/mspencer/ ^^-^^
--
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
--
No virus found in this incoming message.
Checked by AVG Anti-Virus.
Version: 7.0.344 / Virus Database: 267.10.21/96 - Release Date: 9/10/2005
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
--
No virus found in this incoming message.
Checked by AVG Anti-Virus.
Version: 7.0.344 / Virus Database: 267.11.9/116 - Release Date: 9/30/2005
More information about the TheForge