[TheForge] drill bit stock
Larry and Pat Brown
lp.brown at verizon.net
Tue May 31 21:42:09 EDT 2005
Do you have an electric welder? They sell a rod for building up broken
bolts to get them out, The rod burns in the center, under the coating and
doesn't arc to the sides allowing you to puddle a new bolt shaft. Used them
about 4 times with success. Would have used more but that was all that was
in the sample pack. I would try to heat the bit first, then build it up to
where vise grips will help
Larry Brown
At 08:50 AM 5/31/2005 -0700, you wrote:
>Does anyone out there know the type of stock used in the common hardware
>store high speed drill bits for steel. Do you per chance know the steps
>for annealing them.
>
>Yes, I ask because I broke a drill bit in a piece of stock where
>welding, reforging, and repositioning was not an option. I tried all
>the tricks as well as attemting to anneal as I would a common high
>carbon steel and drill it out but it seemed to have little or no affect.
>
>Thank you,
>
>Roger Olsen
>
>_______________________________________________
>Manage membership or unsubscribe at:
>http://mailman.qth.net/mailman/listinfo/theforge
>theforge mail list group photo site is
>http://www.photoaccess.com
>Login: blacksmithblacksmith at hotmail.com
>password: anvil
>___________
More information about the TheForge
mailing list