ed wrote: > Does anyone know who is selling hammer drifts? My old source is no longer > avaiable, and I'm in need of a new one. I suppose I could make it myself, but > I'd rather spend the time making hammers instead of making a new drift. I votefor self made. Grab a hunk of H13 and go... makes a mean drift.