[TheForge] Looking for the cast type hammer drifts...
ed
ed at caffreyknives.net
Mon Mar 21 13:50:42 EST 2005
thanks Ron! I was getting my drifts from a small outfit in Iowa, but their no
longer in business. So now the search is on for another supplier.
Ed Caffrey, ABS Mastersmith
"The Montana Bladesmith"
http://www.caffreyknives.net
ed at caffreyknives.net
---------- Original Message -----------
From: "Ron Childers" <munlaw2 at hcsmail.com>
To: "'Sponsored by ABANA'" <theforge at mailman.qth.net>
Sent: Mon, 21 Mar 2005 12:47:36 -0500
Subject: RE: [TheForge] Looking for the cast type hammer drifts...
> Wendell Machine was selling all sorts of drifts. They are really
> fine folks. Their business is based on the principle that
> blacksmiths are honest people. They don't take plastic - just
> shipped my drifts with an invoice. I'll try to find the address @
> home tonight.
>
> Ron C
>
> -----Original Message-----
> From: theforge-bounces at mailman.qth.net
> [mailto:theforge-bounces at mailman.qth.net] On Behalf Of ed
> Sent: Monday, March 21, 2005 11:44 AM
> To: theforge at mailman.qth.net
> Subject: [TheForge] Looking for the cast type hammer drifts...
>
> Does anyone know who is selling hammer drifts? My old source is no
> longer avaiable, and I'm in need of a new one. I suppose I could
> make it myself, but I'd rather spend the time making hammers instead
> of making a new drift.
>
> Thanks for any help you can offer!
>
> Ed Caffrey, ABS Mastersmith
> "The Montana Bladesmith"
> http://www.caffreyknives.net
> ed at caffreyknives.net
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
------- End of Original Message -------
More information about the TheForge
mailing list