Wayne: I use a Number 8 mesh, with .025, .035 or .045 wire diameter.  Grant
----- Original Message ----- 
From: "Wayne" <longhollow.forge at starband.net>
To: "Sponsored by ABANA" <theforge at mailman.qth.net>
Sent: Friday, March 18, 2005 1:39 PM
Subject: [TheForge] fireplace screen


> Anyone have a good source for fireplace screen?  I found 
> http://www.bwire.com/
> but looking at that site, I'm not sure which type to order.
>
> Wayne