In a nutshell, with outlandish difficulty.
Niobium can be electrodeposited from a molten salt under vacuum. Dow or
DuPont or one of those types patented a process in the mid-seventies. It was used
to plate the internal working of chemical pumps. The process was not pretty.
Hochewa
In a message dated 3/14/2005 9:26:34 AM Eastern Standard Time,
FREEMAB at pt.fdah.com writes:
Niobium jewelry often bears these colors. I wonder whether steel could
be niobium plated?...