[TheForge] Black finish for galvanized

Andrew Vida osan at netlabs.net
Thu Mar 3 10:16:12 EST 2005



RICK KORINEK wrote:
> I am working on an exterior railing that will be installed 
> near the ocean.  I am looking seriously into having it hot-
> dipped.

	A bit late in the game, I suppose, but didn't you consider using stainless?