Phil,
I think that if you harden & temper the dies first then weld them to a
mounting plate that you will loose your temper. Don't you have to pre heat
the thick die material to about 400 degrees before welding?
I also think that there was some discussion about the need for hardening &
tempering dies in the first place. Do you loose your temper when you place
1500 / 2000 degree metal on the dies for an extended period while forging?
These are NOT answers to your questions, just discussion points.
dave mudge
dave at magichammer.net
http://www.magichammer.net
http://www.metalsmithinghowto.com
-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of Phil
Sent: Saturday, June 18, 2005 3:32 PM
To: Sponsored by ABANA
Subject: [TheForge] Sorry to break in with a blacksmithing question
I can't remember what I did before when attaching the
dies to the mounting plates for a kinyon hammer. I'm
using H-13 for the dies.
Should I weld the dies to the mounting plates, and
then harden and temper them, or harden and temper the
dies, and then weld them to the mounting plates?
Once again, sorry for breaking in with a blacksmithing question.
____________________________________________________
Yahoo! Sports
Rekindle the Rivalries. Sign up for Fantasy Football
http://football.fantasysports.yahoo.com
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
More information about the TheForge
mailing list