On May 31, 2005, at 6:55 AM, Bruce Freeman wrote:

> Do ceramic cones come in these temperature ranges?

Yes they do. Check out:

http://www.ortonceramic.com/Resources/Chart-F.pdf

You will probably have to buy direct, few ceramists use use anything  
above cone 10. A *mere* 2350 F :)