[TheForge] Air Hammer Base Plate
Darrell
darrell at machinemaster.com
Thu Jun 9 18:20:42 EDT 2005
I will try to give some useful information.
The 1 1/4" plate will work fine. Just to be sure, figure the cubic inches in
the 1 1/2" plate that is called for and make the 1 1/4" plate large enough
to have the same cubic inches.
Darrell
----- Original Message -----
From: "Dan Tull" <dantull at numail.org>
To: "Sponsored by ABANA" <theforge at mailman.qth.net>
Sent: Thursday, June 09, 2005 2:32 PM
Subject: Re: [TheForge] Air Hammer Base Plate
> You could always add a 1/4" plate.
> ----- Original Message -----
> From: "Phil" <mobjak at yahoo.com>
> To: "Sponsored by ABANA" <theforge at mailman.qth.net>
> Sent: Thursday, June 09, 2005 5:10 PM
> Subject: [TheForge] Air Hammer Base Plate
>
>
> I'm builing the standard size Kinyon, from the ABANA
> plans. The place I get my steel from doesn't have
> 1.5" plate for the base plate. They do have 1.25"
> plate.
> Would that be thick enough?
>
>
>
> __________________________________
> Discover Yahoo!
> Use Yahoo! to plan a weekend, have fun online and more. Check it out!
> http://discover.yahoo.com/
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
More information about the TheForge
mailing list