[TheForge] Re: brill dit stock (grrr)

Bruce Freeman FREEMAB at pt.fdah.com
Thu Jun 2 12:51:52 EDT 2005


If it's not too late, DON'T use play-doh.  Play-doh is salt, water, and cornstarch.  Acid will dissolve it.  You need something water-repellant, like plasticine clay (ordinary kids' toy clay).  You can sift some fine dirt from your yard (clay, not loam) and mix it with a heavy oil (like bar-chain oil) and get something that will do.  No doubt there are lots of other things that will work as well.

Bruce
NJ

>>> sunironworks at yahoo.com 6/2/2005 10:55:33 AM >>>
It's an 8mm bold with about a 6mm extractor in it now. I tried the
dremel approach to dish it out to get a good center punch. Messed up
the top 1/16" of the hole, no big deal. Hope play-doh holds the acid...

J

--- Ron Childers <munlaw2 at hcsmail.com> wrote:

> Justin,
> 
> If all else fails, you should be able to grind the screw extractor
> out with
> a Dremmel Tool. If you mess up the threads, you can repair with a
> Helicoil
> or Keensert, etc. How big is the bolt?
> 
> Ron Childers
> 
> 
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge 
> theforge mail list group photo site is
> http://www.photoaccess.com 
> Login:  blacksmithblacksmith at hotmail.com 
> password:  anvil
> ___________
> 
> 
> 

_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge 
theforge mail list group photo site is
http://www.photoaccess.com 
Login:  blacksmithblacksmith at hotmail.com 
password:  anvil
___________





More information about the TheForge mailing list