Thu Jun 2 10:11:57 EDT 2005
Hello Justin,
I am the one who posed the original question about a broken drill bit and
how to anneal them. Mine was in a bar of 1 inch forged mild steel. I
was hoping to take a heat on the section and anneal as tool steel. What
finally worked for me was drilling from the back side and center
punching, not as simple as it sounds cuz I had already bunged up the hole
from the front side but it did finally work.
My method soes not sound like an option for you but it looks like some
good tips are coming in.
Roger
________________________
Justin Fellenz wrote:
> Roger,
>
> Please share how you got that stud out. A stud just twisted off below
> grade in an aluminum intake manifold I'm working on, so I drilled a
> lovely, perfectly centered hole in the stud and decided--foolish me--to
> try my handy-dandy blue-point screw extractor set, which broke off in
> the *%)#$(#+ hole. So now I have high-carbon steel in a soft steel
> cylinder in aluminum, flush. I can get the broken end of the extractor
> good and red without the aluminum disappearing on me, but obviously
> cant go hotter. I was hoping that I could anneal the extractor by
> keeping the surrounding aluminum warm and then I figgered I'd try my
> own idea of heating the durn thing up and then drilling. The heat runs
> away so fast I ended up drilling while torching and the drill got red
> real fast. Maybe thats the answer though. I'm kind of at an impasse.
>
> Oh, this is a manifold off an old military truck, not the kind of thing
> I want to wreck and have to replace. Goes without saying I suppose.
>
> So...howd'ja do it?
>
> Thanks,
>
> Justin.
>
> --- Roger Olsen <erik at methow.com> wrote:
>
> > Hi Ralph,
> >
> > Thank you for the offer to send over a stick of Stud Plus but I have
> > no need at
> > this time. I solverd my immediatee problem thru stubborness and the
> > sacrifice
> > of other bits. I will definitly keep the Stud Plus in mind and when
> > next at
> > the welding supply by a stick or two. I had never heard of it
> > before.
> >
> > I sure appreciate all this exchange of information and offers of
> > help.
> >
> > Thanks,
> >
> > Roger
> > _________________________
> >
> > Ralph Sproul wrote:
> >
> > > Larry has a good point on this one if the tap is only down about
> > 1/8 of an
> > > inch. This rod is called Stud plus by Allstates repair rods. I
> > have
> > > purchased and used two packages of this rod for removal of broken
> > studs and
> > > bolts from flywheels, dampers, castings, etc.
> > >
> > > I've found the rod does what Larry says and stays to the center if
> > your not
> > > to deep. The flux goes out and fills the threads. On deeper holes
> > where
> > > something is in about 3/8 to 3/4 deep.......I've used a piece of
> > rubber
> > > vacuum hose over the stick to make sure I dont' side arc the
> > threads. When
> > > it is a real critical location I've also used those fibre faucet
> > washers as
> > > "bullseyes" to make sure I hit dead center on the broken stud or
> > bolt with
> > > the rod.
> > >
> > > Roger, do you want me to send along a rod of this material. It is
> > like
> > > 150,018........and it forms up like an icicle - one tack on top of
> > the other
> > > until you can get a grip on the stack of repair rod with a set of
> > vice
> > > grips - or welding on a nut to get a better two sided twist works
> > well also.
> > > So it does not weld up like stud welding - but rather one tack on
> > top of the
> > > next to build it out to where you can get at it.
> > >
> > > Ralph
> > >
> > > ----- Original Message -----
> > > From: "Larry and Pat Brown" <lp.brown at verizon.net>
> > > To: "Sponsored by ABANA" <theforge at mailman.qth.net>
> > > Sent: Tuesday, May 31, 2005 9:42 PM
> > > Subject: Re: [TheForge] drill bit stock
> > >
> > > > Do you have an electric welder? They sell a rod for building up
> > broken
> > > > bolts to get them out, The rod burns in the center, under the
> > coating and
> > > > doesn't arc to the sides allowing you to puddle a new bolt shaft.
> > Used
> > > them
> > > > about 4 times with success. Would have used more but that was all
> > that was
> > > > in the sample pack. I would try to heat the bit first, then build
> > it up to
> > > > where vise grips will help
> > > > Larry Brown
> > > >
> > > >
> > > > At 08:50 AM 5/31/2005 -0700, you wrote:
> > > > >Does anyone out there know the type of stock used in the common
> > hardware
> > > > >store high speed drill bits for steel. Do you per chance know
> > the steps
> > > > >for annealing them.
> > > > >
> > > > >Yes, I ask because I broke a drill bit in a piece of stock
> > where
> > > > >welding, reforging, and repositioning was not an option. I
> > tried all
> > > > >the tricks as well as attemting to anneal as I would a common
> > high
> > > > >carbon steel and drill it out but it seemed to have little or no
> > affect.
> > > > >
> > > > >Thank you,
> > > > >
> > > > >Roger Olsen
> > > > >
> > > > >_______________________________________________
> > > > >Manage membership or unsubscribe at:
> > > > >http://mailman.qth.net/mailman/listinfo/theforge
> > > > >theforge mail list group photo site is
> > > > >http://www.photoaccess.com
> > > > >Login: blacksmithblacksmith at hotmail.com
> > > > >password: anvil
> > > > >___________
> > > >
> > > >
> > > > _______________________________________________
> > > > Manage membership or unsubscribe at:
> > > > http://mailman.qth.net/mailman/listinfo/theforge
> > > > theforge mail list group photo site is
> > > > http://www.photoaccess.com
> > > > Login: blacksmithblacksmith at hotmail.com
> > > > password: anvil
> > > > ___________
> > > >
> > > >
> > >
> > > _______________________________________________
> > > Manage membership or unsubscribe at:
> > > http://mailman.qth.net/mailman/listinfo/theforge
> > > theforge mail list group photo site is
> > > http://www.photoaccess.com
> > > Login: blacksmithblacksmith at hotmail.com
> > > password: anvil
> > > ___________
> >
> > _______________________________________________
> > Manage membership or unsubscribe at:
> > http://mailman.qth.net/mailman/listinfo/theforge
> > theforge mail list group photo site is
> > http://www.photoaccess.com
> > Login: blacksmithblacksmith at hotmail.com
> > password: anvil
> > ___________
> >
> >
> >
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
More information about the TheForge
mailing list