Hey Ralph,
The author said that just about any rod that is small enough to establish an
arc in the hole and weld to the nut without making too large a deposit will
work.
He likes the stainless because it strikes an arc easier and welds at a lower
heat.
He said the L stands for low carbon. The correct rod # is 308L-16.
I find the stainless rod welds easier to most steels; especially alloy
steels ,and with-stands impact better.
I got a can of 316 1/16" rod and find it works well
Chuck
----- Original Message -----
From: "Ralph Sproul" <brhlbsmt at mcttelecom.com>
To: "Sponsored by ABANA" <theforge at mailman.qth.net>
Sent: Thursday, June 02, 2005 5:18 AM
Subject: Re: [TheForge] Re: brill dit stock (grrr)
> Hi Chuck, did the article mention any reason in particular to use a
> stainless rod? I'm curious on that one - cuz I've always used 7018.
>
> 308L is just low carbon stainless, but what is the 16L? Or are they
> suggesting going from low carbon 308 to 316 SS?
>
> (maybe it has something to do with welding strength to the alloys in
> M2?) -
> which would be nice to know.
>
> Ralph
>
> ----- Original Message -----
> From: "Chuck Robinson" <robi5515 at bellsouth.net>
> To: "Sponsored by ABANA" <theforge at mailman.qth.net>
> Sent: Wednesday, June 01, 2005 9:18 PM
> Subject: Re: [TheForge] Re: brill dit stock (grrr)
>
>
>> Hey Justin,
>> I just found the article in the Home Shop Machinist March/April 2004
>> bout
>> removing broken taps and studs.
>> Basically if the tap or stud is close to flush with the surface place
>> the
>> next smaller size nut centered over the hole, reach down with a 1/16"
>> 308L-L16 rod at 65 amps DCEP and weld the stud to the nut
>> It might take a few tries.
>> If the stud/tap is broken further down in the hole, take a next size down
>> bolt, long enough to touch the stud/tap, center drill a hole in it -large
>> enough for the rod to reach the offending part and weld the bolt to it.
>> I also found that a few squirts of Sili-Kroil penetrant really helps.
>> when
>> backing out the bolt.
>> Chuck
>> ----- Original Message -----
>> From: "Justin Fellenz" <sunironworks at yahoo.com>
>> To: "Sponsored by ABANA" <theforge at mailman.qth.net>
>> Sent: Wednesday, June 01, 2005 6:54 PM
>> Subject: Re: [TheForge] Re: brill dit stock (grrr)
>>
>>
>> > Roger,
>> >
>> > Please share how you got that stud out. A stud just twisted off below
>> > grade in an aluminum intake manifold I'm working on, so I drilled a
>> > lovely, perfectly centered hole in the stud and decided--foolish me--to
>> > try my handy-dandy blue-point screw extractor set, which broke off in
>> > the *%)#$(#+ hole. So now I have high-carbon steel in a soft steel
>> > cylinder in aluminum, flush. I can get the broken end of the extractor
>> > good and red without the aluminum disappearing on me, but obviously
>> > cant go hotter. I was hoping that I could anneal the extractor by
>> > keeping the surrounding aluminum warm and then I figgered I'd try my
>> > own idea of heating the durn thing up and then drilling. The heat runs
>> > away so fast I ended up drilling while torching and the drill got red
>> > real fast. Maybe thats the answer though. I'm kind of at an impasse.
>> >
>> > Oh, this is a manifold off an old military truck, not the kind of thing
>> > I want to wreck and have to replace. Goes without saying I suppose.
>> >
>> > So...howd'ja do it?
>> >
>> > Thanks,
>> >
>> > Justin.
>> >
>> > --- Roger Olsen <erik at methow.com> wrote:
>> >
>> >> Hi Ralph,
>> >>
>> >> Thank you for the offer to send over a stick of Stud Plus but I have
>> >> no need at
>> >> this time. I solverd my immediatee problem thru stubborness and the
>> >> sacrifice
>> >> of other bits. I will definitly keep the Stud Plus in mind and when
>> >> next at
>> >> the welding supply by a stick or two. I had never heard of it
>> >> before.
>> >>
>> >> I sure appreciate all this exchange of information and offers of
>> >> help.
>> >>
>> >> Thanks,
>> >>
>> >> Roger
>> >> _________________________
>> >>
>> >> Ralph Sproul wrote:
>> >>
>> >> > Larry has a good point on this one if the tap is only down about
>> >> 1/8 of an
>> >> > inch. This rod is called Stud plus by Allstates repair rods. I
>> >> have
>> >> > purchased and used two packages of this rod for removal of broken
>> >> studs and
>> >> > bolts from flywheels, dampers, castings, etc.
>> >> >
>> >> > I've found the rod does what Larry says and stays to the center if
>> >> your not
>> >> > to deep. The flux goes out and fills the threads. On deeper holes
>> >> where
>> >> > something is in about 3/8 to 3/4 deep.......I've used a piece of
>> >> rubber
>> >> > vacuum hose over the stick to make sure I dont' side arc the
>> >> threads. When
>> >> > it is a real critical location I've also used those fibre faucet
>> >> washers as
>> >> > "bullseyes" to make sure I hit dead center on the broken stud or
>> >> bolt with
>> >> > the rod.
>> >> >
>> >> > Roger, do you want me to send along a rod of this material. It is
>> >> like
>> >> > 150,018........and it forms up like an icicle - one tack on top of
>> >> the other
>> >> > until you can get a grip on the stack of repair rod with a set of
>> >> vice
>> >> > grips - or welding on a nut to get a better two sided twist works
>> >> well also.
>> >> > So it does not weld up like stud welding - but rather one tack on
>> >> top of the
>> >> > next to build it out to where you can get at it.
>> >> >
>> >> > Ralph
>> >> >
>> >> > ----- Original Message -----
>> >> > From: "Larry and Pat Brown" <lp.brown at verizon.net>
>> >> > To: "Sponsored by ABANA" <theforge at mailman.qth.net>
>> >> > Sent: Tuesday, May 31, 2005 9:42 PM
>> >> > Subject: Re: [TheForge] drill bit stock
>> >> >
>> >> > > Do you have an electric welder? They sell a rod for building up
>> >> broken
>> >> > > bolts to get them out, The rod burns in the center, under the
>> >> coating and
>> >> > > doesn't arc to the sides allowing you to puddle a new bolt shaft.
>> >> Used
>> >> > them
>> >> > > about 4 times with success. Would have used more but that was all
>> >> that was
>> >> > > in the sample pack. I would try to heat the bit first, then build
>> >> it up to
>> >> > > where vise grips will help
>> >> > > Larry Brown
>> >> > >
>> >> > >
>> >> > > At 08:50 AM 5/31/2005 -0700, you wrote:
>> >> > > >Does anyone out there know the type of stock used in the common
>> >> hardware
>> >> > > >store high speed drill bits for steel. Do you per chance know
>> >> the steps
>> >> > > >for annealing them.
>> >> > > >
>> >> > > >Yes, I ask because I broke a drill bit in a piece of stock
>> >> where
>> >> > > >welding, reforging, and repositioning was not an option. I
>> >> tried all
>> >> > > >the tricks as well as attemting to anneal as I would a common
>> >> high
>> >> > > >carbon steel and drill it out but it seemed to have little or no
>> >> affect.
>> >> > > >
>> >> > > >Thank you,
>> >> > > >
>> >> > > >Roger Olsen
>> >> > > >
>> >> > > >_______________________________________________
>> >> > > >Manage membership or unsubscribe at:
>> >> > > >http://mailman.qth.net/mailman/listinfo/theforge
>> >> > > >theforge mail list group photo site is
>> >> > > >http://www.photoaccess.com
>> >> > > >Login: blacksmithblacksmith at hotmail.com
>> >> > > >password: anvil
>> >> > > >___________
>> >> > >
>> >> > >
>> >> > > _______________________________________________
>> >> > > Manage membership or unsubscribe at:
>> >> > > http://mailman.qth.net/mailman/listinfo/theforge
>> >> > > theforge mail list group photo site is
>> >> > > http://www.photoaccess.com
>> >> > > Login: blacksmithblacksmith at hotmail.com
>> >> > > password: anvil
>> >> > > ___________
>> >> > >
>> >> > >
>> >> >
>> >> > _______________________________________________
>> >> > Manage membership or unsubscribe at:
>> >> > http://mailman.qth.net/mailman/listinfo/theforge
>> >> > theforge mail list group photo site is
>> >> > http://www.photoaccess.com
>> >> > Login: blacksmithblacksmith at hotmail.com
>> >> > password: anvil
>> >> > ___________
>> >>
>> >> _______________________________________________
>> >> Manage membership or unsubscribe at:
>> >> http://mailman.qth.net/mailman/listinfo/theforge
>> >> theforge mail list group photo site is
>> >> http://www.photoaccess.com
>> >> Login: blacksmithblacksmith at hotmail.com
>> >> password: anvil
>> >> ___________
>> >>
>> >>
>> >>
>> >
>> > _______________________________________________
>> > Manage membership or unsubscribe at:
>> > http://mailman.qth.net/mailman/listinfo/theforge
>> > theforge mail list group photo site is
>> > http://www.photoaccess.com
>> > Login: blacksmithblacksmith at hotmail.com
>> > password: anvil
>> > ___________
>> >
>> >
>> >
>>
>>
>> _______________________________________________
>> Manage membership or unsubscribe at:
>> http://mailman.qth.net/mailman/listinfo/theforge
>> theforge mail list group photo site is
>> http://www.photoaccess.com
>> Login: blacksmithblacksmith at hotmail.com
>> password: anvil
>> ___________
>>
>>
>>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
More information about the TheForge
mailing list