Is there enough meat in the handle stub to drill and tap for a
throughbolt to hold on a nice wooden handle? 

JRF

--- Mike Linn <bamablacksmith at comcast.net> wrote:

> 
> Id grind off the old handle and rivet a new one on..  gotta be
> careful with 
> the riveting because you dont want to crack or break the side wall.
> 
> mike
> 
> 
> At 08:40 AM 7/29/2005, you wrote:
> 
> >I have some old cast iron skillets with the handles broken off with
> about 1"
> >of handle left. Since my daughter likes to cook in these things, I
> thought
> >of making braded and diamond twist handles, weld a short piece of
> black iron
> >pipe and forge it around the original handle stubs. Or does anyone
> know a
> >better way to do it? I thought of grinding the old ones off and
> riveting a Y
> >shaped attachment, but that seems like a lot of work.
> >
> >Ron C
> >
> >_______________________________________________
> >Manage membership or unsubscribe at:
> >http://mailman.qth.net/mailman/listinfo/theforge
> >theforge mail list group photo site is
> >http://www.photoaccess.com
> >Login:  blacksmithblacksmith at hotmail.com
> >password:  anvil
> >___________
> 
> 
>             Mike Linn
>       Artist Blacksmith
>           McCalla, AL
>         AFC Webmaster
> http://afc.abana-chapter.com
> 
>
______________________________________________________________________
> 
> "Many of life's failures are people who did not realize how
>    close they were to success when they gave up. "
>    ~ Thomas A. Edison
>
______________________________________________________________________
> 
> 
> 
> 
> 
> 
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
> 
> 
> 



More information about the TheForge mailing list