[TheForge] Gas Forge Recommendation
Darrell
darrell at machinemaster.com
Fri Jul 22 12:05:18 EDT 2005
Dan,
I think you may be wasting your time making balls for the Whisper Mama.
What makes the balls work is to have the flame coming up through the balls
so the balls absorb the heat.
With the Whisper Mama, the top layer of balls will get hot but the ones
below that layer will be insulated from the flame.
Darrell
----- Original Message -----
From: "Dann" <dann at wctatel.net>
To: "Sponsored by ABANA" <theforge at mailman.qth.net>
Sent: Friday, July 22, 2005 7:39 AM
Subject: Re: [TheForge] Gas Forge Recommendation
> The ceramic thermal mass in a gas forge sounds interesting.
>
> The Melon Ball fruit tool to make up small clay / ceramic balls
> for "heat soaking" ceramics forge welding in a gas forge
> ... brought up a couple thoughts for me. One reason my little
> whisper momma forge heats up so quickly, is that essentially it has
> no thermal mass. The kao-wood lining is very light stuff, but a
> good insulator.
>
> I bought some "anti borax" for gas forge welding, but continue to
> have problems getting a gas forge welds.
>
> Confessions, but even with my coal forge and clean coked
> coal, Getting consistent forge welds is a pain.
>
> So on my "to do" list is to get some cone 8 or so ceramic clay, and
> make up a bunch of little melon balls. I know that they will have to
> be super dry, and probably have to "pre bisk" them in a convention
> oven, as I don't have access to a ceramic kiln. Figure that it
> might be worth the effort to see how the little whisper momma does
> on some sample forge welds, with the firebox semi filled
> with ceramic. If not, well I thought it sounds like a pregnant idea.
>
> Dann
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
More information about the TheForge