[TheForge] Tig welding Stainless

Kenny O. phat at cavenet.com
Fri Jul 1 22:13:37 EDT 2005


it is important that it is clean, match alloys. The right size and color
Tungsten,
in some cases you must have back-up gas. watch your HAZ keep it uniform you
can't
really tell until it cools. but don't let it spread out to much keep a sharp
tip on the Tu
and when you sharpen it keep the tip perpendicular to the grinding surface
so the grinding serrations are parallel to the Tu, not perpendicular.I will
think up more after
I eat.

> > I'm sure there is experience Tig welding Stainless Steel out there. Any
tips?
> >
> > Thanks, Steve