[SCA-Chirurgeon] Fw: [TheForge] Metal Toxicity
Chuck Robinson
robi5515 at bellsouth.net
Mon Jan 31 13:56:20 EST 2005
One that really does work is drinking butter milk after breathing zinc fumes
when welding galvanized steel.
Chuck
More information about the TheForge