[TheForge] forge brazing

magichammer dave at magichammer.net
Sat Jan 29 00:22:08 EST 2005


Wire brush or sand your joints clean.
Copper wire works fine. (striped romex)
Use steel or iron wire to bind your pieces to be brazed.
Apply borax or any other welding flux or blue brazing flux.
Gently heat until copper flows, reduce heat significantly to allow 
solidification.
Remove excess flux when cool.

dave m

Frederick Faller wrote:

>I need some simple suggestions on forge brazing. What
>is a good flux? What is a good brazing material? Can I
>use copper? What sort of surface preparation do I
>need?
>
>Any suggestions or tricks would be helpful.
>
>Frederick Faller
>
>=====
>Frederick W. Faller
>Shiloh Forge Ironware http://users.rcn.com/ffaller/SFI_web.htm
>www.immerland.com
>
>__________________________________________________
>Do You Yahoo!?
>Tired of spam?  Yahoo! Mail has the best spam protection around 
>http://mail.yahoo.com 
>_______________________________________________
>Manage membership or unsubscribe at:
>http://mailman.qth.net/mailman/listinfo/theforge
>theforge mail list group photo site is
>http://www.photoaccess.com
>Login:  blacksmithblacksmith at hotmail.com
>password:  anvil
>___________
>
>
>
>  
>


-- 
No virus found in this outgoing message.
Checked by AVG Anti-Virus.
Version: 7.0.300 / Virus Database: 265.8.2 - Release Date: 1/28/2005



More information about the TheForge mailing list