Bob Ehrenberger wrote: > Kevin, > > Brownell sells a spray on coating that works really well. You spray it on, > let dry, and then bake in the oven. Kind of like parkerising. What do you mean by this? Is it a chemical oxidation thing or a coating that is painted on? Sounds interesting.