[TheForge] conclusion power hammer vs press

Lon Humphrey ironcrossforge at adelphia.net
Fri Jan 21 17:56:28 EST 2005


http://pg.photos.yahoo.com/ph/showyrtits/my_photos
here is that link to my photos

----- Original Message ----- 
From: "Lon Humphrey" <ironcrossforge at adelphia.net>
To: "Sponsored by ABANA" <theforge at mailman.qth.net>
Sent: Friday, January 21, 2005 5:54 PM
Subject: [TheForge] conclusion power hammer vs press


i have decided that i will build a press. now i just have to figure out how 
to suspend the log splitter verticaly in the shop and exhaust the fumes from 
the gass motor.........

any way here is some of my work and my shop

thanks to all who replied info was very helpful

Lon
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login:  blacksmithblacksmith at hotmail.com
password:  anvil
___________






More information about the TheForge mailing list