> >"Rust Bluing" try Birchwood Casey Plum Brown. It is what we use on muzzle
> >loaders.
> Would you mind describing the look of this patina/finish?
It is a brown with just a hint of red and it can be done cold but is a lot
faster if heated in an oven to a couple hundred degrees. Not hot enough to
affect temper.
> Is plum brown a cold process?
> Thanks.
>
> Regards,
> Bill Woolley
>
> >
> >
>
>
>
>