It's on the MFC web site 
http://www.msforgecouncil.com/shop_tip_gallery.htm

 
Jim Pigott


NOTICE: This E-mail (including attachments) is covered by the Electronic
Communications Privacy Act, 18 U.S.C. §§ 2510-2521, is confidential and may
be legally privileged. If you are not the intended recipient, you are hereby
notified that any retention, dissemination, distribution, or copying of this
communication is strictly prohibited. Please reply to the sender that you
have received the message in error, then delete it. Thank you.


-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of Washington, Aubrey O.
Sent: Monday, December 19, 2005 11:48 AM
To: Sponsored by ABANA
Subject: RE: [TheForge] instructions - books, newsletters and websites?

Jim,
What was the story?
 
Aubrey

________________________________

From: theforge-bounces at mailman.qth.net on behalf of Jim Pigott
Sent: Mon 12/19/2005 11:31 AM
To: 'Sponsored by ABANA'
Subject: RE: [TheForge] instructions - books, newsletters and websites?



You're welcome. It originated with a demo and story by Walt Scadden.

 
Jim Pigott
Mississippi Forge Council




-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of Washington, Aubrey O.
Sent: Monday, December 19, 2005 11:03 AM
To: Sponsored by ABANA
Subject: RE: [TheForge] instructions - books, newsletters and websites?

Thanks to whoever suggested the "square knot" wall hook.  I made one last
night and it came out nicely (after a lot of tweaking).

Aubrey

________________________________

From: theforge-bounces at mailman.qth.net on behalf of Mike Linn
Sent: Fri 12/16/2005 7:50 PM
To: Sponsored by ABANA
Subject: Re: [TheForge] instructions - books, newsletters and websites?




Try the "Best of the Bits" vol 1,2,3,4 & 5

available from Judd Clem at Ajc665 at aol.com or 256-232-2615

each is edited by Clay Spencer and is chock full of small to medium
projects & tips

look here for an index of Vol 1 & 2.
http://afc.abana-chapter.com/best_of.html

I havent gotten around to the other volumes yet.

they are:
$14 each
2 for $26
3 for $36
4 for $46
or all 5 for $56
the pricing above includes postage to US addresses

Visa & M/C accepted.. and if you order now you might get them for Christmas.

mike


At 08:11 AM 12/16/2005, you wrote:
>BACKGROUND:
>
>As I'm sure many of you have discovered, when it comes time to demonstrate
>blacksmithing, we often have some difficulty coming up with a good demo
>project.  A good demo, in my opinion, should not take very long, should
>result in an item the audience can relate to or understand, and should not
>involve welding.
>
>(The last is mainly because in demo circumstances - typically full
>daylight - forge welding is difficult.  Another concern is the splash of
>slag hitting the audience, but I don't let that bother me to
>much.  Finally, there's the fear that the weld won't take.  I wouldn't be
>concerned about that at all, except that it IS so hard to judge a weld
>heat in full daylight.  I can routinely make a weld in a shop, but my
>success rate in daylight is dismal.)
>
>My purpose in this is to teach a substantial number of NJBA members each
>some simple demos so that when they show up at a county fair, etc.,
>they'll have something to "show off."
>
>What I'm seeking are good instructions for good projects.  That is to say,
>the instructions must be sufficiently detailed and well illustrated.  This
>proves to be a significant issue.  I've come across many good ideas for
>demo projects, but with little explanation of how to execute them.  While
>I may be able to do it myself, I really don't care to write up a bunch of
>demos right now.  That takes a considerable amount of time and
>effort.  I'd rather make use of demos others have already written up.
>
>I have begun going through my library for projects.  For example, Tucker's
>book is full of interesting projects.  Unfortunately, I doubt I could
>capture an audience's attention with feathers and wedges (rock-splitting
>hardware) for example.  So by the time I get through my list of
>requirements, there are really very few appropriate projects in that
>book.  The same is true for other books I've started going through.  I
>suspect my entire book collection will yield only about a dozen suitable
>projects.
>
>Newsletters are another obvious source of such info, and I plan to go back
>through back-issues I have.  But I have a limited number, so that's a
>limited resource.
>
>Therefore, I'm looking to the Internet for additional demos.  I've already
>gone through AnvilFire and the AFC sites and pulled a few demos from them.
>
>THE QUESTION:
>1) What OTHER websites (ABANA chapters or otherwise) do you know of that
>have project instructions?
>2) What books do you know of with such projects?
>
>Thanks.  Your input is appreciated.
>
>Bruce
>NJ
>
>
>
>_______________________________________________
>Manage membership or unsubscribe at:
>http://mailman.qth.net/mailman/listinfo/theforge
>theforge mail list group photo site is
>http://www.photoaccess.com
>Login:  blacksmithblacksmith at hotmail.com
>password:  anvil
>___________


            Mike Linn
      Artist Blacksmith
          McCalla, AL
        AFC Webmaster
http://afc.abana-chapter.com

______________________________________________________________________

"Many of life's failures are people who did not realize how
   close they were to success when they gave up. "
   ~ Thomas A. Edison
______________________________________________________________________






_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login:  blacksmithblacksmith at hotmail.com
password:  anvil
___________





_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login:  blacksmithblacksmith at hotmail.com
password:  anvil
___________








More information about the TheForge mailing list