Okay, Frosty. I withdraw my crack. (Hmm...that doesn't sound right.)
Anyway, back to the original thread on welding cast iron. I was not able to find any cast iron gas welding rod locally (OKC metro area). But, I did find a dealer that would order less than 50# of Welco Kast Weld 111 for me. He is also ordering the flux. I should hear back from him today.
Aubrey
________________________________
From: theforge-bounces at mailman.qth.net on behalf of frosty at customcpu.com
Sent: Thu 12/15/2005 7:56 PM
To: Sponsored by ABANA
Subject: RE: [TheForge] Brooms and Welding Cast
I'm not sure I like that "experience with Ralph" crack, especially seeing as
you ASSume it.
I have seen pictures though.
<grin>
Frosty
Quoting "Washington, Aubrey O." <awashington at ou.edu>:
> Frosty my man, I'll have to assume that you have had some experience with
> Ralph. (I won't ask what.) So, I will bow...(no, wait, better not bow)...I
> will defer to you greater knowledge and keep Ralph away from my back channel
> in the future.
>
> Aubrey
>
>
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
More information about the TheForge
mailing list