That's it, I was thinking of the scaling chisels. The one you gave me is 
square.

Not only was that a few years ago, I confuse easily. <grin>

Jerry


Quoting schade at acegroup.cc:

> 
> 
> Jer,
> 
> The H13 I don't quench. Just air cool. I do use soybean oil for 
> quenching the scaling chisels that I sharpen for a foundry. Maybe 
> that's what you remember?
> 
> If it's round it's probably H13. If it's square it's probably a piece 
> of one of the foundries chisel (S5). Either one makes a good chisel but 
> the H13 will take more heat.
> 
> Bob
> 